Shimadzu dsc-50 differential scanning calorimeter
| Faculty | Education |
| Department | Chemistry |
| Calibration Status | calibrated |
| Device Type | measuring |
| Device Status | working |
| Maintenance Type | no_maintenance |
| Device Brand | Shimadzu DSC-50 |
| Count of Devices | 1 |
| Device Description | Differential scanning calorimetry (DSC)Samples (3–4 mg) were placed in aluminum pan and heated at a rate of 10 °C/min, with indium in the reference pan, in an atmosphere of nitrogen to a temperature of 400 °C |
| Device Function | it enables the detailed analysis of fusion and crystallization, which is extremely important in selecting material and setting of molding conditions. |